Copper Molybdenum (CuMo)
With Rolling Process
- Thermal conductivity (TC) typically 210 to 255 W/m·K
- Coefficient of Thermal Expansion (CTE) range of 7.2 to 11.0 ppm/K
- Stamped or EDM machined
- Lightweight compared to CuW
- Available in large sheet form
- Metallization options available
Without Rolling Process
- Thermal conductivity (TC) typically 160 W/m·K
- Coefficient of Thermal Expansion (CTE) range of 7.0 ppm/K
- Easily machined
- Lightweight compared to CuW
- Metallization options available
Copper Molybdenum (CuMo)
|